I not sure I understand what you're saying about your customer's
requirement, but appreciate your concern about printing too much paste and
floating the part.
We assemble with EPTSSOP [Exposed Pad Thin Shrink Small Outline Package]
parts, which sounds similar to your part. EPTSSOP increases the thermal
efficiency of power constrained standard TSSOP packages by as much as 150%
by soldering the heat sink pad on the bottom of the package to the board.
Apparently, Amkor [the part fabricator] is particularly optimistic about our
ability to assemble boards with these parts. So, they provide virtually no
information on their site, other than "use standard processes". [er, words
to that effect] We printed various paste volumes, placed, reflowed, and
sectioned dummy parts from Practical Components [probably Top Line and
others have similar parts].
If your customer is asking you to prove that there is solder coverage of the
gold pad for the heat sink after soldering,
* Why not just pop the part off the board with a beer can opener?
* Never tried this, but wont your xray machine show this?
Dave Fish
----- Original Message -----
From: "Andre Leclair" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, October 23, 2001 11:39 AM
Subject: [TN] SMT part with Backside Ground
> Hi All
>
> Hope some one can help? We have have a board from a customer which has a
> PSSop-16 with a Backside Ground ( #RF2119DBP). The stencil house has made
> a cutout that is slightly smaller then the ground on the device. The
> ground plane area on the card is basically the size of the body of the
part
> with 10 via holes in it.
> The customer wants evidance of solder reflow on the ends (Tinning of the
> Gold Plate). Current stencil does not get enough paste to do this and we
> are concerned that if we make the cut out larger then the device contact,
> the part may ride on top of the extra solder and result in
> opens/insufficients on the leads. Also I have been unable to find a
> recomended land/paste pattern for this type of device.
> Any ideas would be appreciated.
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|