Hey Moonman... as far as old technology, we've been building restrained core
technology for nearly 20 years! It started out as polyimide MLBs populated
and then epoxy bonded to Cu-Mo-Cu. We transitioned to silicon carbide
aluminum about 8 years ago, and still use this technology today. It's time
for a change, that's the reason for my post.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Earl Moon [SMTP:[log in to unmask]]
Sent: Tuesday, October 02, 2001 11:57 AM
To: [log in to unmask]
Subject: Re: [TN] Cu-In-Cu boards
Bad hand or no, we did/do some really neat mil/flight DFM stuff. It
almost
is gratifying to know little has changed regarding the
restraining/constraining/tailoring core technology over the past
twenty
years. The big difference now seems only to be the evolution from
CIC to CMC
while realizing they are nearly the same.
Brings back memories concerning the 10 mil copper sheets sandwiched
around
about 40 mils of Invar. Also the 10" maximum panel size comes back
to mind.
Would like to know more about improved processing techniques and how
tailoring core, close to MLB surfaces, compares with constraining
core
useage. Also, what became of Kevlar and/or Carbon fiber technology?
What's really great is to see so many old and new time experts
coming out of
the woodwork. What could this be a sign of? Hope Jame's original
question
didn't get lost. Seems like not.
MoonMan
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|