TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Marsico, James" <[log in to unmask]>
Date:
Tue, 2 Oct 2001 10:37:22 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (119 lines)
Been there...

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879



        -----Original Message-----
        From:   Crepeau, Phil [SMTP:[log in to unmask]]
        Sent:   Tuesday, October 02, 2001 10:23 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] Cu-In-Cu boards

        hi again,

        and oh, by the way, as you must know, lanxide is as brittle as a
ceramic.  which means, it's also embarrassing when the corners that are used
to mount insertion/extraction levers break off.

        phil

        -----Original Message-----
        From: Marsico, James [mailto:[log in to unmask]]
        Sent: Tuesday, October 02, 2001 4:09 AM
        To: [log in to unmask]
        Subject: Re: [TN] Cu-In-Cu boards


        Well, we primarily build military electronics with LCCCs, thus the
need for
        a restrained board. (We're using silicon carbide/aluminum composite
cores.)
        I've been tasked to look at this design/technology and come up with
        alternatives.  I'm interested in alternate restraining core
material, board
        material, leaded SMT components, near-hermetic plastic components,
etc.,
        etc.  What are you military guys/gals doing these days?

        Jim Marsico
        Senior Engineer
        Production Engineering
        EDO Electronics Systems Group
        [log in to unmask] <mailto:[log in to unmask]>
        631-595-5879



                -----Original Message-----
                From:   Earl Moon [SMTP:[log in to unmask]]
                Sent:   Tuesday, October 02, 2001 4:19 AM
                To:     [log in to unmask]; Jim Marsico
                Subject:        Re: Cu-In-Cu boards

                I don't do well at 0200. Maybe you meant thermal-mechamical
        stability. If
                so, CIC obviously applies as does Kevlar and Carbon fiber
materials.
        Diamond
                types are best but anyone up for that?

                I quit, thankfully to us all.

                MoonMan


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2