Provided physical specs of the component will accommodate the wave solder
environment (flux, heat, immersion in molten solder...) they should survive
with no problem.
We currently reflow and wave our devices without issue.
Solder pallets are another possible solution.
Happy to expand on either, off line.
Call with questions.
Richard Elensky
Sr. Manufacturing Engineer
[log in to unmask] <mailto:[log in to unmask]>
Tel: 559-292-1111 x246
Fax: 559-292-9355
Dantel
2991 North Argyle Ave.
Fresno, CA, 93727
Visit our web site at:
http:// www.dantel.com <http://www.dantel.com>
----------
From: Jorge Rodriguez [SMTP:[log in to unmask]]
Sent: Tuesday, October 02, 2001 10:29 AM
To: [log in to unmask]
Subject: [TN] Tantalum Caps
Technetters,
I have a product that has Tantalum Caps, having them waved would
make our
life easier, the board has some TH components we currently hand
solder and
that could be waved. I know that there might be some reason not to
wave
Tantalums, but I am not sure. Can Tantalum Caps be wave soldered?,
Has
anyone done this?
Any responses would be appreciated
Jorge Rodriguez
Process Engineer
Varian Inc
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|