Roger:
I'll take a whack at this.
> Esteemed Colleagues,
> An engineer here wants to reject some SMD assemblies that were assembled
> by
> hand. I have reviewed the A-610, but it doesn't necessarily cover all the
> problems we see. The product has been exhibiting random field failures,
> and some are failing at temperature extremes (-20deg C or +70 to 85deg C).
>
To start with, what did you ask the CM to do? Build em' so they work
or did you specify a workmanship requirement?
> 1) Some pads are missing under a MQPF-144 device. "Former" pads with a
> connection have the lead raised off the board and wire soldered from lead
> to a via under the device. Some unconnected pads are missing and no
> solder
> joint is possible. Accept or reject?
>
Missing pads indicate either really bad circuit boards or a solder
operator who is used to using a jackhammer. Unless you gave the CM the
authority to perform "repairs" as opposed to "rework" I would reject them
all. Again, it depends on what you specified.
> 2) On same device, the wire fix for the removed pad raises the device so
> that the leads had to be bent to the board and then soldered. Looks bad.
> Accept or reject?
>
Anything that looks bad shouldn't be accepted. Anytime a lead needs
to be bent out of the normal shape in order to make a connection is
rejectable. But then again, what did you ask for?
> 3) What are your thoughts about manual SMD assembly with fine pitch parts
> down to 0.5mm for production? (By manual I mean manual part placement and
> manual soldering.)
>
A couple of ways to handle this. Using a hot air tool is a bit more
forgiving than hand soldering with an iron. However, I would only do this on
a limited basis. For a "production" run, NO!
> 4) What are your suggestions as to having our CM improve their soldering
> techniques?
>
Obviously training. But more importantly, finding someone with the
right touch. Even training can't make a watchmaker out of everyone. Identify
those with the talent and go with them.
Hope this helps. Good Luck.
Bill Kasprzak
Moog Inc., Electronic Assembly Engineering
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|