We are using rotary switch encoders on our application and they are failing,
after some were opened, certain kind of yellow grease was found, we are not
sure if that's flux since the encoder is being soldered to the board thru
wave soldering.
After cleaning the "defective" encoder with alcohol the encoder works fine.
Anyone has had a similar experience?? soldering process or encoder supplier
fault??
Please help.
Thanks.
Raúl Valdéz.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|