Hi Glenn! I would add to your list one advantage: 0402's can be
electrically advantageous in RF type circuits; and one disadvantage: an
increased inability to visually inspect the solder joints. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Pelkey, Glenn" <[log in to unmask]>@IPC.ORG> on 08/08/2001 02:55:31
PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Pelkey, Glenn" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Capacitor 0603 vs 0402
Hi all,
I'm brainstorming on risks and benefits of 0603 caps vs 0402 caps.
If the cap value, voltage rating, dielectric material, terminations, and
use conditions are the same, would one be better than the other? My
thoughts are it would be a wash or at least not significant. Here's what I
have so far:
Benefits of 0402 vs 0603:
Smaller size reduces thermal stress/strain on solder joints from CTE or
board flexing.
Smaller size uses less real estate on board
Risks of 0402 vs 0603:
Equipment may have difficulty placing
Thinner dielectric spacing to achieve same capacitance, cap higher failure
rate
Smaller size, cracks easier to develop
Higher risk of tombstoning
What do you all think? I'm sure I missed something, maybe even
wrong on some of the above.
Thanks,
Glenn
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|