TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Tempea, Ioan" <[log in to unmask]>
Date:
Thu, 30 Aug 2001 11:16:49 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (150 lines)
Thanks Grant,

it's also with 0805s that I'm fighting.

What did you do about it?

Ioan

> -----Original Message-----
> From: Grant Emandien [SMTP:[log in to unmask]]
> Sent: Thursday, August 30, 2001 11:02 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Component skew after reflow
>
> Ioan,
>
> You're explaining a similar problem (on 0805's) we had recently (also on
> ENIG boards) - what we noticed was that the applied paste at times was
> offset to one end and further exacerbated by the component being placed
> off-centre to the other end, hence the apparant randomness. Inspection
> prior
> to reflow indicated fractional or no contact between the solder and the
> end.
> This condition resulted in 2 types of defects after reflow i.e. not
> soldered
> at one end (as you mentioned), as well as the more obvious tombstones when
> the tension really gets angry.
>
> Regards
> Grant
>
> -----Original Message-----
> From: Tempea, Ioan [mailto:[log in to unmask]]
> Sent: Thursday, August 30, 2001 4:51 PM
> To: [log in to unmask]
> Subject: [TN] Component skew after reflow
>
>
> Hi Technos,
>
> I have an intriguing one.
>
> I find passive components that are not soldered at one end after reflow.
> These components show very good joints at one extremity while the other
> end
> is not soldered at all. The not soldered end is usually outside of the
> pad,
> at the mercy of the surface tension, but sometimes it touches the
> respective
> pad, being untouched by the solder, that forms nice bumps on the pad.
>
> We're on no-clean paste, the board finish is ENIG. The assembly has being
> running for a long time, we built tenths of thousands without this
> problem.
> But all of a sudden... The problem appears randomly, not always on the
> same
> component, not always at the same place. The frequency is let's say one
> occurence every 50 boards. The assembly is not so populated, barely about
> 50
> parts.
>
> I checked the insertion, it is good. I even offset manually some parts
> before the reflow, but got good soldering on them. The reflow profile is
> the
> same, I even ran the profiler. The paste is OK, good date code, same
> printing conditions, paste height OK. The land patterns are adequate, they
> haven't changed.
>
> First, my instinct told me it's the parts, maybe they're too old. I
> checked
> the reels and the manufacturer's date codes (not the broker's) are between
> mid 2000 until june 2001. Not that old, are they?
>
> What could it be? The board? What and how to check, since the pads are
> very
> well wet? The parts? Anything else?
>
> Thanks for any input,
> Ioan
>
> --------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> --
> -----
>
>
> **********************************************************************
> Notice:
>
> The information contained in this e-mail (including any attachments) may
> contain commercially sensitive or confidential information which may be
> legally privileged and is for the sole use of the intended recipient(s).
> If you are not, or believe you may not be, the intended recipient, you are
> hereby notified that any use, dissemination, copying, review, disclosure
> or action taken in reliance of this e-mail is prohibited and may be
> unlawful. If you have received this message in error, please notify the
> sender immediately by reply e-mail and delete all copies of the message.
>
> Any views expressed in this message are those of the individual sender
> unless expressly stated by the sender to be given on behalf of Tellumat
> (Pty) Ltd. Tellumat (Pty) Ltd disclaims liability for any unauthorised
> opinion or representation made by the sender on behalf of Tellumat (Pty)
> Ltd.
>
> No warranty is given by Tellumat (Pty) Ltd that the integrity or security
> of this e-mail (including any attachments) has been maintained through
> transmission, nor that the communication is free of virus, interception or
> interference.
>
> **********************************************************************
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2