Kathy
It is possible for SOME "no-clean" flux residues to sublimate over time
and then condense elsewhere in a sealed box. This is most likely if the
residues are in the warmest spot and the condensation in the coolest
spot.
Brian
> "Stillings, Kathy" wrote:
>
> A question for the experts...
>
> Is anyone using no-clean on hermetically sealed units? I am running
> into an issue with flux contamination on a few solder joints in a unit
> that contains MIMICs and wedge bonds and is hermetically sealed. The
> flux comes from a couple of magnet wire terminations in the unit. Can
> anyone share some insight?
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------