Gary,
A likely place to find the info you want is the Internationl Tin
Research Institute in the UK - www.itri.co.uk. They have published this
kind of data on a number of solder alloys.
Roger Bilham
In article <[log in to unmask]>, Gary Bremer
<[log in to unmask]> writes
>Can anyone tell me what the properties of Bi14 solder is?
>
>Joint Strength ==>
>Fatigue Resistance ==>
>Yield Strength ==>
>High Temperature Life ==>
>Solder Joints Hardness ==>
>Intermetallic Growth Rates ==>
>Ultimate Tensile Strength ==>
>Percent Elongation ==>
>Adaptability to Stress ==>
>Thermal Fatigue Properties ==>
>Thermal and Electrical Conductivity ==>
>Imtermetallic compounds formed ==>
>
>Could this solder be used in a high reliabilty (class 3) application?
>The application I have is a unit that is subjected to temperatures from -
>40° to + 70° Celsius, vibration of 6G. So far I have conflicting opinions,
>I need some facts and data. I teach soldering and have not heard of anyone
>using this solder within the electronic industry. I check with the
>soldering instructors at China Lake and they had not heard of this solder.
>
>--------------------------------------------------------------------------------
>-
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message: SET Technet
>NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-
>mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>--------------------------------------------------------------------------------
>-
--
Roger Bilham
Roger Bilham Consultancy
Tel: +44 (0)20 8467 8819
Fax: +44 (0)8700 548 613
Mobile +44 (0)7 941 122 446
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|