Ok all you plating guru's.......I am currently specifying a gold
(Thermosonic) wire bondable electrolytic gold for a new board design.
This in my mind was the easy part (Mil G-45204, Type III, Grade A, 40-50
microinches thick). Now for the Nickel, Currently we spec. a
Electrolytic Ni, 4-9% Phos., 150-200 microinches thick.
Questions: Since my bonding is to the gold, is there a concern if the
Ni plating is Electroless or Electrolytic. Which is easier to control ?
Which is a less expensive process ? Any other concerns I should be
aware of ?
Thanks,
Bill C.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|