I agree.
The question was 'as an alternative to HASL".
As an alternative to HASL immersion tin can be very good with all the
benefits mentioned earlier.
One problem to watch out for is compatibility with solder resist - it can
attack some resists causing problems - use a robust resist and you should
see few problems. Like the man said - try it and see what you think.
It's the old horses for courses - immersion gold might be the right finish
for your application but I would definitely try immersion tin first.
Neil
Neil Atkinson
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: 21 August 2001 05:40
Subject: Re: White Tin
Hello folks. Yes it's been a while since i have responded to
any talk on the
net....majority of the time....i like to talk about things i
have experienced
first hand...u know....hands-on.....cuz like they say....
talk is cheap. :o)
For those who aren't aware of the fact.....the company i
work for...has been
marketing white tin for the last 5 years, and our success
speaks for itself.
It amazes me when i see someone asking " does anyone have
info on white tin?"
then getting an answer back...." I would suggest immersion
gold".
Hello!!!!......are we all on the same planet here? If that
someone did try
white tin where immersion gold should have been used in the
first
place.....well.....the answer speaks for itself.
In all my years of working with "white tin" i don't believe
the manufacturers
of the product ever implied that white tin can replace
immersion gold....but
when will people ever sit down and try to understand that
those are two
different applications.....maybe never...and maybe we'll
keep on getting
responses like.......i would suggest immersion gold.
If there are parties interested on more info or references,
please do e-mail
me.........
Thank you for your time
Rich Fudalewski
Florida Cirtech, Inc.
e-mail [log in to unmask]
#####################################################################################
Attention:
This message is for the named person's use only. It may contain confidential,
proprietary or legally privileged information. No confidentiality or privilege
is waived or lost by any mistransmission. If you receive this message in error,
please immediately delete it and all copies of it from your system, destroy any
hard copies of it securely and notify the sender. You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this message
if you are not the intended recipient. STADIUM GROUP PLC and any of its subsidiaries
each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where
the message states otherwise and the sender is authorised to state them to be the
views of Stadium Group Plc. or one of its subsidiaries.
Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate measures on
their systems to intercept any such material.
Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
#####################################################################################
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|