John,
The most pressing question that needs to be answered is "why". The answer will determine the
type, amount, process and testing required.
It is apparent this "encpasulate/potting" requirement is based on some form of end use
problem. The nature and extent of the end use issues will be the determining factor.
David A. Douthit
Manager
LoCan LLC
-------------------------------------
John Fahey wrote:
> I have recently come upon a requirement to encpasulate/pot a small PCB assy
> containing a T/H transformer. Size is approx .5"W x .5"L x .3" H
>
> Can anyone who has experience in "Potting" or "encapsulating"
> technologies ,especially potting PCB assemblies, give me some
> hints/starting points, etc.
>
> I would be very interested in any issues to watch out for, recommended
> potting materials, equipment, standards to adhere to, tests, etc.
> Basically anything that would be helpful.
>
> Thanks in advance,
> John
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|