Scott,
You could reference IPC-6015 or IPC-6016. These address the cleanliness of
the whole board, purity of the metals (by reference to other specs), and
plating thickness. Minimum thickness broken down by class and wire bonding
process. But, I think what the others have said still applies.
Glenn
-----Original Message-----
From: Buscomb, Scott [mailto:[log in to unmask]]
Sent: Monday, July 02, 2001 7:36 AM
To: [log in to unmask]
Subject: [TN] Specs for Wire Bond Pads
I am looking for information on specifying a gold plated surface for wire
bond pads, specifically plating, surface roughness and contamination. Does a
standard industry spec exist? Is there an authoritative text on the subject?
Thanks in advance.
Scott Buscomb
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|