No, he didn't have the assembly covered. He was using the foam like a pot holder while inspecting the circuit board and loaded components.

Thanks for the info. You all have been very helpful!

<<< [log in to unmask]  5/22  6:22a >>>
Neda
It sounds to me like your engineer is folding the foam over the CCA and holding it that way, yes?  Tell your engineer to get out the textbooks and look up "Faraday cage".  If the CCA isn't bagged in a static shielding bag (and the bag closed by folding or ziplock) then all the engineer is doing is pretending to care.

Plus, as has been already noted, the board should be handled by the edges.  

Our standard for moving boards anything more than a few dozen feet is to have it bagged, and the bag put in an envelope of pink bubblewrap.  Perhaps overkill but better safe than sorry.

http://www.esda.org/ for the Electrostatic Discharge Association - more info there.

Good luck, and bring a big stick!

regards

Graham Collins
Process Engineer, Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215

>>> [log in to unmask] 05/21/01 02:30PM >>>
** High Priority **

Hello everyone! I need help settling a dispute. I am aware of the fact that the pink foam designed for packing esd sensitive assemblies helps eliminate the possibility of a charge being generated during a transport while cushioning the product but I have an engineer telling me that the assemblies are safe if holding  the assembly in hand while ungrounded as long as the foam separates the hand at the point the pcb is held. If someone knows this to be true please send me more information on this because this contradicts what I have always been taught and what I am teaching. I need your help ASAP!

TIA, Neda

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

                        

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2