IPC-SM-785, Guidelines for Accelerated Reliability Tests, Werner E. (SMT,
that is)
served me well Luca, just instead of silver polymer bridging (fails more
than solder)
use very fine copper links (caps, (dipped in paste prior reflow), for event
detector loops.
Best use Yo own production board, chained -up, not keen on test vehicles.
paul
-----Original Message-----
From: Luca Amato [mailto:[log in to unmask]]
Sent: Tuesday, May 29, 2001 12:54 AM
To: [log in to unmask]
Subject: [TN] Temperature cycling specification
Can anybody provide me with a reference to a standard specification for
solder joint reliability test with particular reference to fatigue tests
(temperature cycling table etc.)?
Luca
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|