Genny,
If you received boards that had a tin finish it is more than likely White
Tin Immersion. I cannot speak for all chemical vendors but I know ours has
been tested for whiskering and passed easily. You can retrieve the
information we have compiled on our web site at: www.floridacirtech.com You
will find an independent lab study done by Trace Labs addressing your
question regarding whiskers.
Our white tin is called "Omikron" other vendors are selling tin under
different names some better than others, It does matter which tin you use and
of course the board house has to apply it correctly. You can e-mail me
directly if you have any questions, chances are I can help you with this
issue.
Steve Wentz
Florida CirTech
408-202-9329
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|