A couple considerations on solder peaks including what Kathy said about
potential breakoffs, would be arching, and if it's RF you may have other
problems with interference/cross talk, and if it is built into a final
assembly the chance may be there for shorting. Solder peaks are normally
not the preferred condition of the final joint.
Ron Hollandsworth
ITT
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|