Hi JS!
The IPC has a standard in which to do this. It's under the IPC-TM-650, Method
2.4.37.2. It provides a means to measure and evaluate soldering tool
performance by using a standard technique and using a defined copper clad
coupon. One of the criteria is heat recovery...
-Steve Gregory-
<< Hi TechNetters,
I want to evaluate some soldering systems and need to compare the heat
recovery of the iron tips. I have no experience in this. Do you guys know
of a standard method and equipment of measuring the temperature vs time of
the solder iron tip during rework? Thanks.
Rgds,
JS >>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------