I know of an n-methyl pyrrolidinone based stripper that also contains
HCFC-141B that will strip polyurethane conformal coatings. The labels says
it will attack polystyrene, ABS and acrylic. It also says not to store near
heat sources or aluminum. Contact me off-line for more info.
Tim Reeves
|-----Original Message-----
|From: Marsico, James [mailto:[log in to unmask]]
|Sent: Thursday, May 03, 2001 4:38 AM
|Subject: ACRYLIC CONFORMAL COATING CLEANING SOLUTION
|
|
|Hello Technet:
|Not seeing any stars or stripes today (maybe an occasional
|pink elephant,
|though). I'm looking for a non-flammable, non-toxic material
|which can be
|used in a dip tank (or cold spray) to remove acrylic conformal
|coating from
|holding/masking fixtures. Any suggestions?
|Jim Marsico
|Senior Engineer
|Production Engineering
|AIL/Electronics Systems Group
|An EDO Company
[log in to unmask] <mailto:[log in to unmask]>
|
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|