Steve: It depends on the type of epoxy you are trying to remove, the amine's
are usually the toughest. Also, if it's a room temp cure you may have a shot
at it, if it's a two part bake cure your probably out of luck. It is very
difficult if not impossible to strip off epoxy ink without attacking the
soldermask or resin in the laminate.
Dynaloy Inc. makes a variety of epoxy strippers PHN# 800-669-5709. Most of
these are heated and messy to work with, can you mechanically abrade off the
ink?
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, March 20, 2001 7:37 AM
To: [log in to unmask]
Subject: [TN] Epoxy Ink Stripper...
Hi ya'll!
Everybody got their "MIR" helmets on? They say now that it'll be Friday when
they plan to "De-orbit" the space station...
Anyways, could anybody give me a recommendation on a good solvent (or
whatever), to use to remove cured epoxy ink. It's for when there's a mistake
been made serializing PCB's...
As always, thanks in advance...
-Steve Gregory-
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|