TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 21 Feb 2001 10:06:04 -0600
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (686 bytes) , TEXT.htm (1519 bytes)
Good Morning, 
Is the non-soldered termination slightly lifted? 0402's in my experience have a tendenancy to lift if the pad layout isn't right.
Have you performed any solderability tests of the suspect parts to determine solderability?

Hope it helps.

Kathy

>>> [log in to unmask] 02/19/01 10:00PM >>>

Hello,
 
Does anyone have solderability issues with 0402 capacitors? We adjusted our reflow profiles a few times according to different manufacturers but so far have not completely resolved the problem. What we noticed was no-soldered of terminal(s) at random locations, and didn't appear to be manufacturer specific.
 
Any suggestion on how to approach this?
 
Regards.
 
Peter


<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN">
<HTML><HEAD>
<META content="text/html; charset=iso-8859-1" http-equiv=Content-Type>
<META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD>
<BODY style="FONT: 8pt Arial; MARGIN-LEFT: 2px; MARGIN-TOP: 2px">
<DIV><FONT size=1>Good Morning, </FONT></DIV>
<DIV><FONT size=1>Is the non-soldered termination slightly lifted?&nbsp; 0402's
in my experience have a tendenancy to lift if the pad layout isn't
right.</FONT></DIV>
<DIV><FONT size=1>Have you performed any solderability tests of the suspect
parts to determine solderability?&nbsp;</FONT></DIV>
<DIV>&nbsp;</DIV>
<DIV><FONT size=1>Hope&nbsp;it helps.</FONT></DIV>
<DIV><FONT size=1></FONT>&nbsp;</DIV>
<DIV><FONT size=1>Kathy&nbsp; </FONT><BR><BR>&gt;&gt;&gt; [log in to unmask]
02/19/01 10:00PM &gt;&gt;&gt;<BR></DIV>
<DIV><FONT size=2>Hello,</FONT></DIV>
<DIV><FONT size=2></FONT>&nbsp;</DIV>
<DIV><FONT size=2>Does anyone have&nbsp;solderability&nbsp;issues with&nbsp;0402
capacitors? We adjusted our reflow profiles a few times according to different
manufacturers but so far have not completely resolved the problem. What we
noticed was no-soldered&nbsp;of terminal(s) at random locations, and didn't
appear to be manufacturer specific.</FONT></DIV>
<DIV><FONT size=2></FONT>&nbsp;</DIV>
<DIV><FONT size=2>Any suggestion on how to approach this?</FONT></DIV>
<DIV><FONT size=2></FONT>&nbsp;</DIV>
<DIV><FONT size=2>Regards.</FONT></DIV>
<DIV><FONT size=2></FONT>&nbsp;</DIV>
<DIV><FONT size=2>Peter</FONT></DIV></BODY></HTML>