Good Morning, Is the non-soldered termination slightly lifted? 0402's in my experience have a tendenancy to lift if the pad layout isn't right. Have you performed any solderability tests of the suspect parts to determine solderability? Hope it helps. Kathy >>> [log in to unmask] 02/19/01 10:00PM >>> Hello, Does anyone have solderability issues with 0402 capacitors? We adjusted our reflow profiles a few times according to different manufacturers but so far have not completely resolved the problem. What we noticed was no-soldered of terminal(s) at random locations, and didn't appear to be manufacturer specific. Any suggestion on how to approach this? Regards. Peter