Hi Werner,
I will try to still your curiosity. Sending you some delicate pictures
offline. Hope you cope with the views, so I don't get blamed for sending too
upsetting pictures. Is there possibly a 'Playboy' also for soldering? Can
imagin a midpage in Circuit World showing exciting IMCs and etched
samples?...He-he.
Have a nice day and avoid lead poisoning
Ingemar
PS. Will check in Wassink and AWS's handbook.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: den 21 januari 2001 03:33
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] squashed pancakes
Hi Ingemar,
You did not give the thermal history, but to get "Ni/Tin IMC is many
microns"
thick you need to sit at high temperatures for a long time--not just one or
2
reflows. Just look up the Ni-dissolution rate in Sn in Klein-Wassink. I
would
love to see those pictures together wioth the history.
Werner Engelmaier
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|