In a message dated 1/24/01 1:20:24 PM Central Standard Time,
[log in to unmask] writes:
<< As you know, underfill is rarely used for higher pitch BGA (1mm or
1.27mm). Unfortunately, I've lent my proceedings to someone, so I can't give
you much detail.
Hope this helps.
Charles Elliott >>
Hi Charles!
That's what I'm learning, from everything that I've been reading from the
stuff I'm finding on the web (when talking about underfill), are mostly
dealing with flip-chip, or other CSP packages...
Yes, when dealing with CSP's and flip-chips, it has been shown that
underfilling increases the reliability (depending on what you read), two to
four fold...
So the next big question is; is it REALLY necessary to underfill standard
pitch BGA's? Maybe our customer has seen the data for flip-chips and CSP's
and feel that if it helps with these packages, it must also help with
standard pitch BGA's. Our customer is a defense supplier by the way...
What I have learned is that if you want to increase BGA reliability, use PCB
materials that have low CTE's...that's where the real problem is, since BGA
solder joints aren't as compliant as gull-wing joints...
I have learned that our customer hasn't really spec'd out a material yet,
researching the rework-ability of different materials...I've learned that is
a pretty big consideration, whether the material is thermo-setting, or
thermo-plastic...
I've got so much to learn!
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|