Hi Ryan,
We electroplate tin-lead then shoot them through the reflow oven. We use
Shipley Ronal chemistry and run DC at 12.5 amps per square foot for 22
minutes or 25 minutes for thicker boards (~150 mils).
Don't know when we'd have to be worried about being lead free.
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials Engineer (Process & Manufacturing)
Warner Robins Air Logistics Center
Avionics Production Division
Precision Attack/ Radar/Manufacturing Branch
Engineering Section
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
-----Original Message-----
From: Ryan Jennens [mailto:[log in to unmask]]
Sent: Friday, September 22, 2000 3:01 PM
To: [log in to unmask]
Subject: Re: [TN] Component Taping Equipment?
We use the V-tek machines also. Much, much better than tubes. We
find it
much more economical becuase the placement accuracy is much better.
On a separate note, I know this topic has been on Technet before,
but does
anybody electroplate tin/lead, rather than HASL? Is it common? If it is
not done, why not?
The reason this comes up is that we get bare boards in here with
soldermask
plugging (capping, tenting) the topside vias and test points. Solder from
the HASL process invaraibly plugs some bottom side vias/testpoints. When
they pass through the reflow oven, boom, solderballs. I understand why this
is happening, so to relieve the trappped air/flux residue/etc., we spefified
that the topside vias/testpoints be left open with 20-mil opening in the
soldermask. Now, when we send the boards through, we don't get solder
balls, but some (a few) vias form a drip that is adhered to the annular ring
of the via and is difficult to remove. Stencil gasketing is then nearly
inpossible. While these occur much less frequently than the solder balls, a
plating process would not plug holes like HASL does. So, rather than having
to choose the lesser of two evils, is plating possible?
-Ryan Jennens
TelGen Corporation
(517) 887-6666 x151
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen R. Gregory
Sent: Friday, September 22, 2000 2:16 PM
To: [log in to unmask]
Subject: Re: [TN] Component Taping Equipment?
In a message dated 09/22/2000 12:20:07 PM Central Daylight Time,
[log in to unmask] writes:
> As a small contract manufacturer, we receive alot of components that
aren't
> machine placeable from our customers. I'm looking into the possibility
of
> putting the components on tape and reel in-house. Any feedback on
vendors
> for this equipment and the feasability/cost effectiveness of doing this
> would be appreciated. Should I even consider it or just send parts out?
>
> Thanks in advance,
>
>
> Rick Thompson
> Ventura Electronics Assembly
> 2665A Park Center Dr.
> Simi Valley, CA 93065
>
> +1 (805) 584-9858 voice
> +1 (805) 584-1529 fax
> [log in to unmask]
Hi Rick!
We've got a V-Tek machine here...it's a model that I don't think they make
any more...it's called a Compak. It's manual but we don't do any high-volume
tape and reeling. I like it because the set-up is so easy. Uses PSA
(pressure
sensitive adhesive) cover tape, so you don't have to worry about heat shoe
settings or things of that sort...
Go to:
http://www.vtekusa.com/products.htm
There will be their latest models there...they're not that expensive either.
Like I said we don't do any high volume taping, so it fits our needs pretty
good.
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|