Hi Shirley,
You could always verify for drilled hole diameter, wicking and nodules with
a microsection. Of course this works best after plating and can be inspected
as per IPC-6012 and IPC-600. You will also get a general idea of the
roughness just by looking at it still on a microsection, this can be checked
on the section prior to plating, but there are no IPC standards for it.
P.S. Wicking is best seen on a non-metallographic microscope wit a good
depth of field.
Hope this helps,
Alain Savard, B.Sc.
Chemical Process Analyst
CAE Electronics Ltd.
e-mail: [log in to unmask]
-----Original Message-----
From: Shirley Xiao [mailto:[log in to unmask]]
Sent: August 3, 2000 5:32 AM
To: [log in to unmask]
Subject: [TN] Hole wall roughness
Is there anyone knows how to measure hole wall
roughness after drilling or after plating? (Notes:I've
searched TechNet archive but there is nothing about
hole wall roughness.)
Thanks and best regards
Shirley
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|