Hi all,
I have been noticing on our last batch of boards that we ran, some of the
tsop flash chips were not reflowing properly. I am not getting very good
toe fillets on the chips and some appear as though they are just sitting on
top of the reflowed solder. This board has a good component mix(i.e. BGA,
QFPs, PLCCsocket, SOICs, total(325-350)). Other components reflow fine,
but for some reason these TSOPS are not. Is there something that we are
overlooking?
Your input would be greatly appreciated. Thanks in advance
Tom
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|