Werner-
T-260 is a time to delamination test, a sample is heated at 10 or 20 C/ min
and held at 260 C until there is a catastrophic failure (delam), the time
is calculated, and gives a relative sense of how well the parts were
processed.
At 19:23 6/14/2000 EDT, you wrote:
>Hi Mark,
>I have been around for a long time but have never heard of a "T260" test.
>What exactly do you mean by this?
>Werner Engelmaier
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
Ian A. McMillan
Engineer
Herco Technology
Ph# 858-679-2800 ext. 107
Fax# 858-679-7565
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|