They have two large circular pads (like about .750") that they use as battery
contacts. He says that this is the place that he has corrosion risk. I can't tell if
the corrosion risk is from battery leakage or environmental effects. Anyway, he says
that corrosion significantly impacts the battery life.
ralph
David Hillman wrote:
> Hi Ralph! Can you provide more information on what the customer
> considers/experienced "corrosion" and what type of use environment he/she
> was talking about?
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
> Ralph Richart <[log in to unmask]>@IPC.ORG> on 06/08/2000 11:55:26 AM
>
> Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
> to Ralph Richart <[log in to unmask]>
>
> Sent by: TechNet <[log in to unmask]>
>
> To: [log in to unmask]
> cc:
>
> Subject: [TN] still confused
>
> We have answers....
>
> So I had a long talk with my customer this morning to provide input
> based on the invaluable advice from you all.
>
> I said - "is there a specific reason for choosing 3-8u" of immersion
> gold over tin/lead solder?"
> He said - "absolutely, the gold provides corrosion resistance, the gold
> does not"
> I said - "even such a thin amount - only 3-8u"?"
> He said - "definitely, all we need is the coverage, the thickness is
> irrelevant"
>
> Is this true?
>
> Needless to say, we are rebuilding the parts as we speak. Rework sounds
> difficult to say the least, although I may try to come up with some
> scheme for fun as they have a bunch of boards that are no good right
> now.
>
> thanks for all the help.....
>
> ralph
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|