One recent gotcha with 4oz Cu we had was using Dry Film Soldermask on top of
it - I believe the term is "soda strawing". The copper was too tall for the
dry film to conform too, leaving a gap/pocket adjacent to copper. This was
the customers design ... Steve G. had fun with this one.