You can measure the ionic contamaination levels. An Omegameter works well.
Jim Gilbert
-----Original Message-----
From: Poh Kong Hui [SMTP:[log in to unmask]]
Sent: Wednesday, May 31, 2000 10:56 AM
To: [log in to unmask]
Subject: [TN] Measurement of flux residue
Hi all Technetters,
I would like to know is there any way to measure the flux
residue that left on the board, after wave-soldering process.
Thanks in advance.
Regards,
Poh
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|