hi,
it seems that the rogers corporation makes silicone foams. i would also check with dow corning.
phil
-----Original Message-----
From: Paul Klasek [mailto:[log in to unmask]]
Sent: Monday, April 17, 2000 11:05 PM
To: [log in to unmask]
Subject: [TN] Foamed Silicon
Dear Netties ,
i'm seriously stuck here ;
could any of you spare me ANY lead (non Pb) to foamed flexible silicon
please :
the target is hydrolysis
(humidity/temperature aging, of foamed polyurethanes for example)
resistant flexible foam , inject mouldable to curing dies ;
about 50 grams shot size (a handful, 6"ball)
Technology, equipment, sheet/block fabricators, .......
The foamed silicon lasts for a century ; unlike pu for less than decade .
I realize 'm stretching it here on Net with a bit distant subject ;
appreciate the help .
Thanks a lot
Paul Klasek
http://www.resmed.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|