TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Phil Crepeau <[log in to unmask]>
Date:
Tue, 18 Apr 2000 08:18:06 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Crepeau <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
hi,

it seems that the rogers corporation makes silicone foams.  i would also check with dow corning.

phil

-----Original Message-----
From: Paul Klasek [mailto:[log in to unmask]]
Sent: Monday, April 17, 2000 11:05 PM
To: [log in to unmask]
Subject: [TN] Foamed Silicon


Dear Netties ,
i'm seriously stuck here ;
could any of you spare me ANY lead (non Pb) to foamed flexible silicon
please :

the target is hydrolysis
(humidity/temperature aging, of foamed polyurethanes for example)
resistant flexible foam , inject mouldable to curing dies ;
about 50 grams shot size (a handful, 6"ball)

Technology, equipment, sheet/block fabricators, .......

The foamed silicon lasts for a century ; unlike pu for less than decade .

I realize 'm stretching it here on Net with a bit distant subject ;
appreciate the help .

Thanks a lot

Paul Klasek
http://www.resmed.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2