WRBE-.35ISOBRY-0BA
151,569.50
22ga 12/.21 BE ISO6722B
WRBE-.5ISOBRY-0AC
27,386.80
20ga 19/.19 BE ISO6722B
WRBE-.75ISOBRY-0AC
0
18ga 19/.23 BE ISO6722B
WRBE-01ISOBRY-0AC
64,267.00
16ga 19/.27 BK ISO6722B
WRBE-03ISOBRY-0BA
3,080.37
12ga 44/.31 BE ISO6722B
WRBE-2.5ISOBRY-0AD
78,435.00
2.5 37/0.28 BE ISO6722B
WRBE-2.5ISOBRY-0BA
18,406.00
2.5 50/.26 BE ISO6722B
WRBK-.35ISOBRY-0AB
109,018.00
22ga 7/.26 BK ISO6722B
WRBK-.75ISOBRY-0AC
6,534.80
18ga 19/.23 BK ISO6722B
WRBK-.75ISOBRY-0BA
63,460.00
18ga 24/.21 BK ISO6722B
WRBK-01ISOBRY-0AC
37,026.00
16ga 19/.27 BK ISO6722B
WRBK-02ISOBRY-0AC
21,413.00
14ga 19/.38 BK ISO6722B
WRBK-04ISOBRY-0BA
29,382.00
76783111K ( 04 ISOBRY-0BA BK )
WRBK-05ISOBRY-0BA
8,092.72
10ga 65/.33 BK ISO6722B
WRBK-06ISOBRY-0BA
8,598.48
76783121K (06 ISOBRY-0BA BK)
WRBK-10ISOBRY-0BA
6,840.55
FMV0091000
WRBK-2.5ISOBRY-0AD
40,954.00
2.5 37/0.28 BK ISO6722B
WRBK-25EXRADHV
8,869.92
EXRAD EF1250-25
WRBK-35EXRADHV
6,108.68
EXRAD EF1250-35
WRBN-.35ISOBRY-0BA
184,228.00
22ga 7/.26 BN ISO6722B
WRBN-.5ISOBRY-0AC
75,302.00
20ga 19/.19 BN ISO6722B
WRBN-.75ISOBRY-0AC
51,683.90
18ga 19/.23 BN ISO6722B
WRBN-02ISOBRY-0AC
8,293.37
14ga 19/.38 BN ISO6722B
WRGN-.35ISOBRY-0BA
152,393.50
22ga 12/.21 GN ISO6722B
WRGN-.5ISOBRY-0AC
32,364.05
20ga 19/.19 GN ISO6722B
WRGN-.75ISOBRY-0AC
4,616.46
18ga 19/.23 GN ISO6722B
WRGN-.75ISOBRY-0BA
0
18ga 24/.21 GN ISO6722B
WRGN-2.5ISOBRY-0BA
19,862.00
2.5 50/.26 GN ISO6722B
WRGY-.35ISOBRY-0AB
46,489.29
22ga 7/.26 GY ISO6722B
WRGY-.35ISOBRY-0BA
96,686.00
22ga 7/.26 GY ISO6722B
WRGY-.5ISOBRY-0AC
146,817.00
20ga 19/.19 GY ISO6722B
WRGY-.75ISOBRY-0AC
80,561.00
18ga 19/.23 GY ISO6722B
WRGY-02ISOBRY-0AC
33,572.00
14ga 19/.38 GY ISO6722B
WROE-.35ISOBRY-0BA
34,171.30
22ga 7/.26 OE ISO6722B
WROE-.5ISOBRY-0AC
0
20ga 19/.19 OE ISO6722B
WROE-.75ISOBRY-0AC
23,525.26
18ga 19/.23 OE ISO6722B
WRPE-.35ISOBRY-0BA
204,062.40
22ga 12/.21 PE ISO6722B
WRPE-.5ISOBRY-0AC
30,765.15
20ga 19/.19 PE ISO6722B
WRPE-.75ISOBRY-0AC
51,815.39
18ga 19/.23 PE ISO6722B
WRPE-02ISOBRY-0AC
53,367.00
14ga 19/.38 BK ISO6722B
WRPE-1.5ISOBRY-0AC
36,430.00
1.5 19/.33 PE ISO6722B
WRPE-2.5ISOBRY-0BA
19,329.00
2.5 50/.26 PE ISO6722B
WRPK-.5ISOBRY-0AC
28,705.37
20ga 19/.19 PK ISO6722B
WRPK-.75ISOBRY-0AC
57,224.00
18ga 19/.23 PK ISO6722B
WRPK-.75ISOBRY-0BA
74,136.00
18ga 24/.21 PK ISO6722B
WRPK-01ISOBRY-0AC
31,606.00
16ga 19/.27 BK ISO6722B
WRRD-.5ISOBRY-0BA
85,992.00
20ga ISOBRY-0BA 16/0.21 RD
WRRD-.75ISOBRY-0AC
14,070.00
18ga 19/.23 RD ISO6722B
WRRD-01ISOBRY-0AC
27,049.24
16ga 19/.27 BK ISO6722B
WRRD-02ISOBRY-0AC
49,251.00
14ga 19/.38 RD ISO6722B
WRRD-03ISOBRY-0BA
79,835.70
12ga 44/.31 RD ISO6722B
WRRD-04ISOBRY-0BA
368.587
76783111K ( 04 ISOBRY-0BA RD )
WRRD-05ISOBRY-0BA
2,823.87
10ga 65/.33 RD ISO6722B
WRRD-06ISOBRY-0BA
8,169.00
76783121K (06 ISOBRY-0BA RD)
WRRD-10ISOBRY-0BA
10,783.11
FMV0091000
WRRD-2.5ISOBRY-0AD
74,375.00
2.5 37/0.28 RD ISO6722B
WRRD-25EXRADHV
2,092.13
EXRAD EF1250-25
WRRD-35EXRADHV
5,075.02
EXRAD EF1250-35
WRWE-.5ISOBRY-0AC
98,112.00
20ga 19/.19 WE ISO6722B
WRYW-.35ISOBRY-0BA
110,262.26
22ga 7/.26 YW ISO6722B
WRYW-.5ISOBRY-0AC
159,526.00
20ga 19/.19 YW ISO6722B
WRYW-.75ISOBRY-0AC
18,839.26
18ga 19/.23 YW ISO6722B
WRYW-01ISOBRY-0AC
65,969.00
16ga 19/.27 YW ISO6722B
WRYW-03ISOBRY-0BA
28,973.00
12ga 44/.31 YW ISO6722B
WRYW-2.5ISOBRY-0AD
33,044.00
2.5 37/0.28 YW ISO6722B
WRYW-2.5ISOBRY-0BA
24,134.00
2.5 50/.26 YW ISO6722B
########################################################################
Access the WHMAXSINVENTORY Home Page and Archives:
http://listserv.ipc.org/scripts/wa.exe?A0=WHMAXSINVENTORY
Unsubscribe from the WHMAXSINVENTORY List:
http://listserv.ipc.org/scripts/wa.exe?SUBED1=WHMAXSINVENTORY
WHMA/IPC offers this listserv as an industry benefit but does not control the site and disclaims all liability for its content. Your interactions with organizations and/or individuals found on this site, including payment and delivery of goods or services, are solely between you and such organizations and/or individuals. By using this site, you hereby agree to release WHMA/IPC, its officers, employees, and agents from claims, demands and damages of every kind or nature.
########################################################################
|