Picture 2 looks like copper dissolution. You may have exposes the copper ring pad to the wave too long time.
Suggest to reduce the contact time with solder wave.
________________________________
From: TGAsia [mailto:[log in to unmask]] On Behalf Of WTSZ-Anny Zhou
Sent: Tuesday, March 11, 2008 1:17 PM
To: [log in to unmask]
Subject: [TGA] 转发: Discrepant Material Report #IRR-08 0088 Requires Disposition.
Dear All,
有谁帮我看看附件上的几幅图片,什么情况下可能会造成如此锡裂?谢谢!
________________________________
发件人: WTSZ-WenLi Mao
发送时间: Tuesday, March 11, 2008 12:22 PM
收件人: WTSZ-Anny Zhou
主题: 转发: Discrepant Material Report #IRR-080088 Requires Disposition.
FYI
________________________________
________________________________
Important Notice: This message is intended only for use by the addressee(s) and may contain information that is privileged and confidential. If you are not the intended recipient(s), you are hereby notified that any form of disclosure, distribution, copying or use of this communication is strictly prohibited and may be unlawful. If you have received this communication in error, please notify us immediately by reply and delete the email and destroy any copies of it. This email is for information purposes only and is not intended to nor will it create any binding legal relations. Wong's International (Holdings) Limited. <http://www.wongswih.com>
Legal Disclaimer:
The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
|
|
|