Dennis,
I think you are referring to MIL -STD -202,G, method 208G - solderability.
Right ? Based on this standard, section2.0, it cites that the
solderability test for the components should be done according to
J-STD-002. This method 208G directly make reference to J-STD-002. Thus,
there is no difference in the procedure for carrying the solderability test
of component 's termination. However, you have to check the updated ver.
of J-STD-002 from IPC website
Regards,
Jackson Chan
Technical Services Manager
Cookson Electronics - Alpha Metals
Dennis Cheung
<dennis.cheung@SA
MTEC.COM> To
Sent by: TGAsia [log in to unmask]
<[log in to unmask]> cc
Subject
2008/01/10 ¤W¤È [TGA] MIL STD 202 vs J-STD-002
10:15
Please respond to
Asia Committe
Task Group Forum
<[log in to unmask]>;
Please respond to
Dennis Cheung
<dennis.cheung@SA
MTEC.COM>
Dear all,
Would you like to advise the different between MIL standard and J standard
that caption above? Up to my understanding, MIL STD 202 cover different
test standard for electronics components, where J-STD 002 specify on the
solderability. If it is true, any different between the solderability test
method and requirement that stated in MIL and J-STD?
Regards,
Dennis
Dennis CHEUNG - Regional Field Application Engineer
SAMTEC HONG KONG LIMITED
Phone: (852)26904858 Direct Line: (852)22524402
Fax: (852)26904842
Email: [log in to unmask]
WebSite: www.samtec.com
Above quote is valid for 90 days from date of quote unless otherwise
stated. Price & lead time varies for different quantity and is subject to
material availability & production capacity.
To place an order, please call 852-26904858 to speak with a Customer
Service Representative, FAX PO to 852-26904842 or email at [log in to unmask]
If you use Samtec products without an ACD series part number in the
automotive industry or in other applications having specific requirements,
then you agree that you will not use these products in automotive scorecard
evaluations and agree that you will waive Samtec¡¦s obligations under TS
16949 or any customer specific requirements. Go to www.samtec.com/TS for
details.
Cancellation and Return Guidelines can be viewed at www.samtec.com/terms.
|
|
|