Subject: | |
From: | |
Reply To: | |
Date: | Wed, 20 Jul 2011 11:42:47 +0800 |
Content-Type: | multipart/related |
Parts/Attachments: |
|
|
Dear Jima,
從不良外觀看,不是包覆形狀處也有吃錫不良情形,不良很可能源於pin的表面處理,或者鍍層太薄導致底材氧化,或者鍍層夠厚,電鍍品質不良造成的.
________________________________
From: TGAsia [mailto:[log in to unmask]] On Behalf Of David Lau
Sent: Wednesday, July 20, 2011 11:06 AM
To: [log in to unmask]
Subject: Re: [TGAsia] D-Sub ConnectorPin 吃錫不良
Jima,
本人认为根本原因来自pin脚形状和镀层,建议剪短脚(小于0.8mm)过炉焊接观其效果.
Regards!
David Lau
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Jima Hsieh [謝國偉]
Sent: 2011年7月20日 10:37
To: [log in to unmask]
Subject: [TGAsia] D-Sub ConnectorPin 吃錫不良
各位同業先進
下面這種包覆式的Pin腳的D-Sub Connector在過波焊爐(Wave Soldering)時幾乎都會有吃錫不良現象
我司製程已調整過Flux、Conveyer速度調整過無法改善,機板其他位置吃錫狀況都沒問題,工程初步判定是零件原材問題
但因為此零件每批投產在縫隙處方幾乎吃錫狀況都不好,這樣吃錫異常是否有可能是的包覆式Pin腳設計造成的?
不知各位是否有遇到相同的狀況?(這樣的吃錫無法符合焊接起始面引腳與孔璧吃錫須達270°的要求)
請大家不吝賜教,謝謝
吃錫不良1
[cid:[log in to unmask]]
吃錫不良2
[cid:[log in to unmask]]
原材外觀
[cid:[log in to unmask]]
Best Regards,
Jima Hsieh
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
DISCLAIMER:
*************************************************************************************************************************
This email message, including any attachments, is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies of the original message. [Delta Electronics (Jiang Su) Ltd.]
*************************************************************************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|