TGASIA Archives

October 2010

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
zrf[张仁富] <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, zrf[张仁富] <[log in to unmask]>
Date:
Thu, 28 Oct 2010 15:26:05 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
各位前辈高手,

请教一款柔性板 :板材与金各占成品板子的百分比是多少。。



板子情况:

一层板,板材是台虹的 THKS100520JY ,板材中 PI为:   1mil      AD为:20UM,   CU为: 0.5oz

表面处理是沉金

完成板子的尺寸是长  3.91MM
宽 2.54MM
厚  0.06MM



先感谢了



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2