TGASIA Archives

March 2011

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Asia Committe Task Group Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 17 Mar 2011 08:22:01 +0800
Reply-To:
Asia Committe Task Group Forum <[log in to unmask]>, Patricia Lui <[log in to unmask]>
Subject:
From:
Patricia Lui <[log in to unmask]>
In-Reply-To:
Content-Type:
multipart/alternative; boundary="0-1824494700-1300321321=:9804"
MIME-Version:
1.0
Parts/Attachments:
text/plain (3298 bytes) , text/html (5 kB)
Thanks Evan and Tom for your advices.

--- On Wed, 16/3/11, TL Zhang <[log in to unmask]> wrote:


From: TL Zhang <[log in to unmask]>
Subject: [TGAsia] 答复: [TGAsia] 回覆: [TGAsia] leadfree hand soldering t emperature
To: [log in to unmask]
Date: Wednesday, 16 March, 2011, 9:42 AM




Excuse me, what do you mean temperature is too low? Do you mean the hand soldering temperature? Does this can solve the problem of pads lift? 
Hi,Liu,if your customer have to use hand soldering rework, I advice you use LFmaterial of Tg150 or Tg170. 

Evan 







Tom Zhang <[log in to unmask]> 
发件人:  TGAsia <[log in to unmask]> 
2011-03-16 08:49 




请答复 给
Asia Committe Task Group Forum <[log in to unmask]>; 请答复 给
[log in to unmask]






收件人
[log in to unmask] 


抄送



主题
[TGAsia] 回覆: [TGAsia] leadfree hand soldering t emperature









Temperature is too low  I advise temperature setted  380+(-)10 degC. 
  
Best regards 
Tom Zhang (张涛)
Customer Service Department 
FIC (Suzhou) Inc.
Tel: +86 512 62581988 Ext:5629
Fax:+86 512 62581973
Email:[log in to unmask] 
  



寄件者: TGAsia [mailto:[log in to unmask]] 代理 Patricia Lui
寄件日期: 2011年3月15日 23:17
收件者: [log in to unmask]
主旨: [TGAsia] leadfree hand soldering temperature




Dear Sir, 
  
I have a customer who often complains boards supplied by us have pads lift issue when they do hand soldering rework. This customer is using hand soldering with temperature set at 320-349 degC for leadfree soldering rework and the boards supplied by us are with Tg130-140 degC only. We hope to have your expertise advice what is the common leadfree hand soldering temperature and if need to withstand 320-349degC hand soldering temperature, what Tg material should be used. 
  
Hope to receive your favourable advise. 
  
Thanks & Best Regards 
Patricia Lui 
Xuan Technologies


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________ 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2