TGASIA Archives

June 2007

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Perry <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, John Perry <[log in to unmask]>
Date:
Thu, 7 Jun 2007 10:03:51 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (88 lines)
The only B-24 test board providers that I am aware of are here in the United States.  

IPC maintains a web listing of those IPC member companies who can provide prefabricated versions of the IPC-B-24 test board at:

http://www.ipc.org/ContentPage.aspx?PageID=4.4.3

Alternately, IPC provides the electronic Gerber artwork files that can be used to fabricate this test board.  That is available from IPC as IPC-A-24-G-KIT.  

Regards,

John Perry
Technical Project Manager
IPC
3000 Lakeside Drive # 309S
Bannockburn, IL 60015
[log in to unmask]
1-847-597-2818 (P)
1-847-615-7105 (F)
1-847-615-7100 (Main)

-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Laya Chen
Sent: Wednesday, June 06, 2007 9:33 PM
To: [log in to unmask]
Subject: [TGA] 答复: [TGA] IPC-B-24 Test PCB

Hi Sky,

As Dave stated, Microtek has over 20 years history of providing testing services to the PCB and PCBA industries. We provide SIR, CAF, ECM testing services at out our Changzhou, Jiangsu facility.

There are no current official IPC-B-24 board suppliers at current time, but we are trying to becoming one. And we should be able to supply them soon.

Microtek Changzhou's contact information:
Name: Microtek (Changzhou) Laboratories 麦可罗泰克(常州)实验室
Address: 中国江苏常州新北区电子科技产业园新科路19号
电话:0519-5487805 陈燕

Best regards,
Laya Chen  陈燕
Microtek (Changzhou) Laboratories
Tel: +86 519 5487805
Cell: +86 13115289328
Fax: +86 519 5487810 
Email: [log in to unmask]
-----邮件原件-----
发件人: TGAsia [mailto:[log in to unmask]] 代表 David Bergman
发送时间: 2007年6月7日 10:00
收件人: [log in to unmask]
主题: Re: [TGA] IPC-B-24 Test PCB

Hi Sky,
 
I know that Microtek in Changzhou can do this test.  Maybe Bob or Laya at Microtek know a local source of coupons.
 
David W. Bergman, CAE
Vice President, Standards, Technology and International Relations
IPC
3000 Lakeside Drive # 309S
Bannockburn, IL 60015
Phone 847-597-2840 Fax 847-615-5640
Mobile 847-867-1388
Main 847-615-7100
email [log in to unmask]      www.ipc.org

________________________________

From: TGAsia on behalf of Sky He
Sent: Wed 6/6/2007 8:09 PM
To: [log in to unmask]
Subject: [TGA] IPC-B-24 Test PCB



Hei, Everybody,

I am looking for some IPC-B-24 test comb board to do SIR test. Anyone can help on this or provide supplier information.

PS: is there any lab in Shanghai able to do SIR test?

 