康生,陈生,
对于电子元器件的镀层厚度测量,XRF进行非破坏性量测,Cross Section进行破坏性量测,库伦法适应于较薄、厚度较均匀的镀层厚度量测。下面几个镀层厚度的国标供参考,摘录自《电子产品三防技术手册》,马骖等编著:
GB4956-85 磁性测量法,误差小于10%或1.5um的最大值。
GB4957-85 涡流测量法,误差±10%。
GB11250.2-89 X射线光谱测量法,最大测量厚度15um,等效于ASTM-B568-91。
GB5931-86 β射线反向散射法。
GB8015.2-87 光切显微法。
GB5928-86 溶解法。
GB4955-85 库仑法。
GB5929-86 金相显微法。
GB11378-89 轮廓仪法。
ISO3868-76 干涉显微镜法。
ASTM还有一个关于镀层厚度的测量方法,标号忘记了,呵呵。
Peter Deng
**************************************************
Reliability Lab
Electrical & Electronics
Consumer Testing Services
SGS Shenzhen branch
Tel + 86 0755-26710624
Mobile + 86 13828768267
Fax + 86 0755-26710594
Email [log in to unmask]
Website www.sgs.com/ee
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Jackson Chan
Sent: 2007年7月24日 13:52
To: [log in to unmask]
Subject: Re: [TGA] 请教
Hi LF,
For PCB, I know that different specification is established for different
surface finish
I quote here some related standards
IPC-4552 : ENIG
IPC-4553: Im Ag
IPC-4554: Im Sn
EDS - XRF (non-destructive method) is one of method to measure the
thickness. Certainly, the cross section (see IPC-TM-650 2.1.1) should be
capable , in conjuction with the etching technique if applicable.
Besides, IPC 6010 series specifiesthe plating thickness for different type
of boards.
Regards,
Jackson
lhkang
<[log in to unmask]
CN> To
Sent by: TGAsia [log in to unmask]
<[log in to unmask]> cc
Subject
2007/07/24 上午 [TGA] 请教
10:49
Please respond to
Asia Committe
Task Group Forum
<[log in to unmask]>;
Please respond to
lhkang
<[log in to unmask]
CN>
各位,
请教一下, 有没有关于电子器件(包括PCB)镀层的测试方面的标准?谢谢!
康来辉(LHKang)
Information in this email and any attachments is confidential and
intended solely for the use of the individual(s) to whom it is addressed
or otherwise directed. Please note that any views or opinions presented
in this email are solely those of the author and do not necessarily
represent those of the Company.
Finally, the recipient should check this email and any attachments for
the presence of viruses. The Company accepts no liability for any damage
caused by any virus transmitted by this email.
All SGS services are rendered in accordance with the applicable SGS
conditions of service available on request and accessible at
http://www.sgs.com/terms_and_conditions.htm
|
|
|