请教大家一个问题: LED灯防UV老化的等级是多少? IPC规范有没有定义?或是在其他的
标准上有没有谈到?
Sunny
Amphenol
Tel: 86-20-3483-9838
Fax: 86-20-3483-9800
Email: [log in to unmask]
_____
发件人: TGAsia [mailto:[log in to unmask]] 代表 Justin Wu
发送时间: 2010年3月8日 星期一 10:26
收件人: [log in to unmask]
主题: Re: [TGAsia] Soldering reliability test method standard
Hi Alex,
Maybe you can refer to IPC-9701: Qualification and Performance Test Methods
for Surface Mount Solder Attachments or IPC-SM-785: Guidelines for
Accelerated Reliability Test of Surface Mount Solder Attachments.
Thanks and best regards,
Justin Wu
Utilux South China Ltd
Phone: +86-755-2850 7521
Fax: +86-755-2850 0927
E-mail Address: [log in to unmask]
www.utiluxchina.com
_____
From: TGAsia [mailto:[log in to unmask]] On Behalf Of 浩海 ?
Sent: Sunday, March 07, 2010 1:18 PM
To: [log in to unmask]
Subject: [TGAsia] Soldering reliability test method standard
Dear everyone,
Do you know which standard is about the soldering reliability test method?
Thank you!
张浩海
Alex Zhang
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|