大哥大姐,你们发这个邮件能不能不要BCC给我?
我都不知道你们是发错了还是怎么搞的那也不用BCC吧!!!!!!
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Petrel Pang
Sent: Friday, April 22, 2011 10:57 AM
To: [log in to unmask]
Subject: Re: [TGAsia] 检验标准确认
Hi Sherry,
了解到有些公司用30%,有些用50%作管控,供参考。
应考虑零件的作用,可以和客户协商规定。
Thank you with Best Regards!
Petrel Tel: 86-756-5322318
________________________________
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Sherry Ma
Sent: Friday, April 22, 2011 9:55 AM
To: [log in to unmask]
Subject: Re: [TGAsia] 检验标准确认
Hi Sonic
零件焊接后没有偏移,只是在X-RAY检验时发现有空洞现象,所以想请教一下,这类元件焊接后空洞的判定标准为多少?
Thanks!
Sherry
________________________________
From: Sonic Lu [mailto:[log in to unmask]]
Sent: Friday, April 22, 2011 09:31
To: [log in to unmask]
Subject: Re: [TGAsia] 检验标准确认
1.BGA的气泡标准不是IPC-A-610
2.BGA的气泡标准是IPC-7095
3.没有焊球的就不能用BGA的标准
4.建议还是使用IPC-A-610,以零件焊接后是否偏移以及偏移的多少为判定标准
Thanks and Best Regards
Sonic Lu 陆尚
Process Engineer
Autoliv Electronics China (ACE) Co.,Ltd
Tel: +86-21-67109300-3162
Sherry Ma <[log in to unmask]>
Sent by: TGAsia <[log in to unmask]>
2011-04-22 08:36
Please respond to
Asia Committe Task Group Forum <[log in to unmask]>; Please respond to
Sherry Ma <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
[TGAsia] 检验标准确认
Dear all:
向各位请教一下,如图所示的零件(零件下没有焊球),像这类零件是否可以按IPC-A-610上BGA的标准来检查焊接气泡。
如果不能用BGA的焊接要求来判定的话,我们应该用什么标准来判定呢?
Regards!
Sherry
Legal Disclaimer: The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|