,您好!
请参考 IPC 610E 9.3
2011-11-10
李志民
公司:烽火通信科技股份有限公司
部门:系统设备制造部 电子装联车间
电话:027-67840140
传真:027-67840143
地址: 湖北省武汉市 东湖高新技术开发区东信路5号
邮箱: [log in to unmask]
发件人: 王云峰
发送时间: 2011-11-10 11:48:28
收件人: [log in to unmask]
抄送:
主题: [TGAsia] 回复: Re: [TGAsia]贴片绕线圈塑料体破损的标准
经过测试性能没有影响,而且线圈本来就是暴露在空气中。无法说服供应商。请问有无相关的判定标准?
-------------------------------------
Ivon Wong
Engineering Department
Wuhan Telecommunication Devices Co., Ltd.
Tel: (+86)13886135361
Mobile: (+86)18071040166
Email: [log in to unmask]
Date 2011-11-10
发件人: sonic.lu Thanks c Lu陆尚 Process Engineer Autoliv Electronics China (ACE) Co.,Ltd Tel: +86-21-67109300-3162 *************************************************************** Consider the environment before printing this mesage.
发送时间: 2011-11-10 08:52
收件人: [log in to unmask]
抄送:
主题: Re: [TGAsia]贴片绕线圈塑料体破损的标准
不行咯,零件表面破损,已经露出零件内部结构,3F已经不能满足,拒收
Thanks and Best Regards
Sonic Lu 陆尚
Process Engineer
Autoliv Electronics China (ACE) Co.,Ltd
Tel: +86-21-67109300-3162
王云峰 <[log in to unmask]>
Sent by: TGAsia <[log in to unmask]>
2011-11-09 19:21 Please respond to
Asia Committe Task Group Forum <[log in to unmask]>; Please respond to
王云峰 <[log in to unmask]>
To<[log in to unmask]>
cc
Subject[TGAsia] 贴片绕线圈塑料体破损的标准
大家好!
公司内部关于贴片绕线圈塑料体破损的标准有分歧,在610E内也查不到针对性的标准,请问以下两种情况是否在接受范围内(2级产品)?
-------------------------------------
Ivon Wong
Engineering Department
Wuhan Telecommunication Devices Co., Ltd.
Tel: (+86)13886135361
Mobile: (+86)18071040166
Email: [log in to unmask]
Date 2011-11-09
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
***************************************************************
Consider the environment before printing this message.
To read Autoliv's Information and Confidentiality Notice, follow this link:
http://www.autoliv.com/disclaimer.html
***************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|