suggest to consult with OSP supplier to get some suggestions.
or set DOE to define appropriate temperature and time.
>>> Roger Liu <[log in to unmask]> 2008-8-27 14:23
>>>
低温长时间,和高温短时间是否有一个对应关系表?
Best Regards!
Roger Liu
NG ENG GUAN <[log in to unmask]>
Sent by: TGAsia <[log in to unmask]>
08/27/2008 02:18 PM
Please respond to
Asia Committe Task Group Forum <[log in to unmask]>; Please respond to
NG ENG GUAN <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TGA] PCB silksreen issue
低温烘烤就行了。。没必要高温。。。
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: 27 August 2008 13:07
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TGA] PCB silksreen issue
In my plant, the same as Cony Su point of view normally
OSP板不得烘烤后使用
From: TGAsia [mailto:[log in to unmask]] On Behalf Of NG ENG GUAN
Sent: Wednesday, August 27, 2008 12:54 PM
To: [log in to unmask]
Subject: Re: [TGA] PCB silksreen issue
可以烘烤啦。。。。只是效果不理想。。。有很多dry solder.
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Cony Su
Sent: 27 August 2008 11:25
To: [log in to unmask]
Subject: Re: [TGA] PCB silksreen issue
OSP PCB 不能烘烤的
Best Regards
Cony Su
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Roger Liu
Sent: Wednesday, August 27, 2008 11:18 AM
To: [log in to unmask]
Subject: Re: [TGA] PCB silksreen issue
Team,
We bake the OSP PCB board, but the color was changed. Who can help what
the problem happened? Can we still use them as normal?
Best Regards!
Roger Liu
Office: (086) 022-25293662