TGASIA Archives

March 2010

TGAsia@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Liu <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, James Liu <[log in to unmask]>
Date:
Mon, 1 Mar 2010 22:31:54 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Hi Lewis,

All hot air gun have their sensors. Generally, the probe is located in the center of hot air outlet.

In 7711/21, the temperature is not mandatory. There is a way to confirm the temperature with a piece of paper. You can find it in followed steps.



Best Regards,



James Liu 刘春光

Director, Technology & Standardization 技术与标准总监

IPC China

上海市长宁区延安西路1088号2303室

Suite 2303,#1088 West Yan'an Rd., Changning, Shanghai 200052 PRC

Tel:   +86 21 5497 3435

Fax:  +86 21 5497 3437

MP:   +86 136 0133 3491

[log in to unmask]<mailto:[log in to unmask]>

www.ipc.org.cn<http://www.ipc.org.cn/>



2010年3月份上海



________________________________

发件人: TGAsia [[log in to unmask]] 代表 Lewis Liu [[log in to unmask]]

发送时间: 2010年3月2日 12:03

收件人: Listserv TGAsia

主题: [TGAsia] measure the hot air temperature method



Hi,All:

In IPC 7721 and 7711 document just mentioned the hot air temperature  is approximately 425℃ and adjust it if necessary ,but it didn’t define the test method to get the real  temperature.

Do you have the relative solutions?

Thanks,



Lewis Liu (刘定豪)

Engineering Department

Failure Analysis laboratory Supervisor

Tel:+86<tel:+86> -25- 52728710

Cell:+86 -25 -13851527451

Mail:  [log in to unmask]<mailto:[log in to unmask]>

Kimball Electronics (Nanjing) Co.,Ltd





______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]

______________________________________________________________________


ATOM RSS1 RSS2