Hello All,
Our production line is currently encountering a problem, one of our
components(0402 ESD suppressor) sticks on the cover tape during our SMT
procedure(see below picture). The defect rate exceeds 30%.
We suspected the reason for this failure is due to Static caused. The
static may be produced by friction between cover tape and SMT feeder.
Is there anybody here saw similar problem and what is the reason caused
the failure?
Is any standard/requirement/range for the material surface resistance
for the cover tape and carrier tape?
The test result from the supplier is: carrier tape surface
resistivity---<106, Cover tape surface resistivity--- 0.9~4.08*109.
Is the result acceptable?
Is there any impact to the product because of this issue?
Thanks for your response...
Best regards,
Scott Li
Creating value that increases customer competitiveness
Building 1, 2, 3, Yusheng Industrial Park
467 Xixiang Section, National Highway 107,
Baoan District, Shenzhen, Guangdong, PRC
518126
+86 755 8947 6447 direct
+86 189 2377 9881 mobile
+86 755 8947 6666 fax
[log in to unmask] <mailto:[log in to unmask]> I
www.flextronics.com <http://www.flextronics.com>
Legal Disclaimer:
The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|