	Steve: Try Aremco Products Inc.(914)762-0685.They make a variety of	
	electrically conductive adhesives that use Ag,Ni or C depending on 
	the amount of conductivity required.They have epoxy systems that will	
	go to 320 C intermittent and ceramic ones that will go to over 600 C.	
	Good Luck!							
					Regards				
					Michael Barmuta			
					Fluke Corp.			
					Everett Wa.			
					(206)356-6076		
On Thu, 14 Nov 1996 14:21:37 -0800 [log in to unmask] wrote:

> From: [log in to unmask]> Date: Thu, 14 Nov 1996 14:21:37 -0800
> Subject: Elec. Cond. Adhesive for Hi Temp
> To: [log in to unmask]
> 
> Is there an electrically conductive adhesive which will survive a reflow 
> at 220-240 C while maintaining reasonable bond strength?  Probably not, 
> but I thought I'd ask anyway.
> 
> 
> [log in to unmask]
> ph:503-359-9300 ext. 54653
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to:           *
> * [log in to unmask] with <subject: unsubscribe> and no text.        *
> ***************************************************************************
> 



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2