TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 10 Apr 2000 08:35:49 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Douglas Pauls <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
In a message dated 04/10/2000 7:06:42 AM US Eastern Standard Time,
[log in to unmask] writes:

>
>  What level of conductivity in water do you accept if you use water to
rinse
> boards in an inline cleaner? In IPC-AC-62A p 12 the recommended level is 1
> microsiemens/Cm if one is to conformally coat the boards afterwards.

We recommend the use of deionized water in all aqueous cleaning operations.
For us, deionized water is 2.0 megohm-centimeters of resistivity or higher.
Being metrically challenged, I am not sure what that is in microsiemens per
centimeter.

Doug Pauls
CSL

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2